rec.sport.unicycling · Public discussion

Anodising

Started by tobbogonist · · Last activity · 13 posts · 235 views

This thread is locked and is currently read-only.

Thread navigation

Jump through the discussion

Go to the original post, the replies on this page, or the latest preserved contribution.

Thread details

What we know about this thread

Original section
rec.sport.unicycling
Published
8 February 2007
Last activity
15 February 2007
Original author
tobbogonist
Posts
13
Discussion status
Public discussion
Total views
235
Views / 30 days
0

The navigation and discussion metadata provide context. Posts remain in their original chronological order.

Showing posts 1–13 of 13
Posts remain in their original chronological order.

Text size
  1. I searched and found a few threads about anodising but none of them
    actually came to a conclusion. Did anyone anodise anything? and is it
    possible to anodise my KH frame? after sandblasting all that lovely
    blue off of course. I am hinking of calling around and trying to get a
    quote, but i was just wondering if anyone has done it before and if it
    is worth it?

    I have a friend who can do it in his backyard but he is leaving for
    university in a week, he got a scholorship in Sydney.

    --
    tobbogonist

    I like flies, there the only thing in the world that can make a grown
    man hit himself in the head.
    ------------------------------------------------------------------------
    tobbogonist's Profile: http://www.unicyclist.com/profile/12176
    View this thread: http://www.unicyclist.com/thread/57702

  2. Isn't the KH frame CroMoly? You can anodize aluminum, not steel. If it's
    CroMoly it's a steel alloy and you're out of luck. Put a magnet on it
    and see if it sticks. If so, you're not going to be anodizing it.

    --
    harper

    -Greg Harper

    B L U E S H I F T

    *jc is the only main man. there can be no other.*
    Finally made it to my (n+1)th post....* TOTALLY AWESOME!!!*

    Quoted message said:

    <> Unicycle For the Chafing <><


    ------------------------------------------------------------------------
    harper's Profile: http://www.unicyclist.com/profile/426
    View this thread: http://www.unicyclist.com/thread/57702

  3. harper said:

    Isn't the KH frame CroMoly? You can anodize aluminum, not steel. If it's
    CroMoly it's a steel alloy and you're out of luck. Put a magnet on it
    and see if it sticks. If so, you're not going to be anodizing it.

    KH frames have been aluminum since 2005.

    --
    Spencer Hochberg

    'BC wheel movie.'
    (http://www.unicyclist.com/forums/showthread.php?t=56195) Watch
    it.
    'Bedford Unicycles' (http://BedfordUnicycles.ca)
    AIM: SpencerHochberg
    Email: Litldude2 (at) aol (dot) com

    Cody keeps messing with my sig line...
    ------------------------------------------------------------------------
    Spencer Hochberg's Profile: http://www.unicyclist.com/profile/12659
    View this thread: http://www.unicyclist.com/thread/57702

  4. It is deffinitely possible to anodise any of the blue KH frames, infact
    the blue colour is anodising. You will need to shot blast it back to
    bare metal, and you will loose the KH signatures and KH 20/24/29 logo
    on the neck, as these are areas that are bare metal and when you
    anodise again they will be covered like the rest of it.

    --
    kington99

    Dave

    - what a thoroughly post-modern subversion of the cycling genre -
    ------------------------------------------------------------------------
    kington99's Profile: http://www.unicyclist.com/profile/9417
    View this thread: http://www.unicyclist.com/thread/57702

  5. i'm interested too to know how to do that...

    --
    bobousse
    ------------------------------------------------------------------------
    bobousse's Profile: http://www.unicyclist.com/profile/11961
    View this thread: http://www.unicyclist.com/thread/57702

  6. bobousse said:

    i'm interested too to know how to do that...

    Well in short, go to a local anodising shop and give them some money.
    You can anodise at home, but you'll need various equipment and salts,
    and a big tub. I've seen sets of this equipment for doing small parts
    and they're atleast £100, compared to maybe £20 to get it done
    professionally it's not really worth it, and you'd have to get it
    shotblast somewhere unless you have your own compressor and blast gun
    too.

    --
    kington99

    Dave

    - what a thoroughly post-modern subversion of the cycling genre -
    ------------------------------------------------------------------------
    kington99's Profile: http://www.unicyclist.com/profile/9417
    View this thread: http://www.unicyclist.com/thread/57702

  7. ok so i think that i'll probably go to a shop
    thanks for the information
    bobousse

    --
    bobousse
    ------------------------------------------------------------------------
    bobousse's Profile: http://www.unicyclist.com/profile/11961
    View this thread: http://www.unicyclist.com/thread/57702

  8. i would think powdercoating woul dbe nicer though, just a thought...
    even pro anodising.. well its not as good as a nice powdercoat...

    --
    brendan
    ------------------------------------------------------------------------
    brendan's Profile: http://www.unicyclist.com/profile/13680
    View this thread: http://www.unicyclist.com/thread/57702

  9. kington99 said:

    It is deffinitely possible to anodise any of the blue KH frames, infact
    the blue colour is anodising. You will need to shot blast it back to
    bare metal, and you will loose the KH signatures and KH 20/24/29 logo
    on the neck, as these are areas that are bare metal and when you
    anodise again they will be covered like the rest of it.

    i thought they were powdercoated

    --
    Chris.James

    "Thats my favorite thing about unicycling, I can eat oreos while
    riding!" ~Me

    "Darwin was once of the greatest minds of our time!...Then why is he
    making out with Satan?" ~The Simpsons

    "I'm riding a unicycle with my pants down...this should be every boy's
    dream!"~Bart Simpson
    ------------------------------------------------------------------------
    Chris.James's Profile: http://www.unicyclist.com/profile/14072
    View this thread: http://www.unicyclist.com/thread/57702

  10. I anno all my uni's with a blue to black fade, sometimes I'll have
    another color in the "fade zone".

    --
    mrwhitechristmas
    ------------------------------------------------------------------------
    mrwhitechristmas's Profile: http://www.unicyclist.com/profile/14336
    View this thread: http://www.unicyclist.com/thread/57702

  11. Anodizing is a pretty durable coating for aluminum. It is not immune to
    fading over time though. It is essentially a controlled oxide coating
    of the aluminum that does have a measurable build up. It'll will add
    about .0005-.0010" of thickness everywhere. It is important that the
    anodizing shop plug or mask all of the threaded holes and precision
    bearing surfaces so that they don't get anodized. I've never looked
    closely at a KH frame to know just how precision the bearing surfaces
    are. My guess is, not enough to worry about. The thing to watch for
    is the threaded holes. Most anodizing shops know to mask the threaded
    holes but it's still best to make sure they do this. I've seen some
    who just throw the parts in their vat and don't pay any attention to
    this. The anodized finish gets into the threads and then you can't get
    the bolts in. The surface is hard enough to make it a real bear to try
    and clean the threads up with a tap. I've broken taps off in the hole
    trying to clean up anodized threads before. And then, trying to get a
    broken tap out of a hole can be damn near impossible.

    That's all. Good durable finish that will fade over time and you gotta
    watch the precision machined areas. Pretty colors available.

    --
    underdog

    'I tell you, we are here on Earth to fart around, and don't let anybody
    tell you different' - Kurt Vonnegut
    ------------------------------------------------------------------------
    underdog's Profile: http://www.unicyclist.com/profile/6197
    View this thread: http://www.unicyclist.com/thread/57702

  12. sweet, thanks for the help.
    i have rung around and obtained some quotes for sandblasting and the
    cheapest i found is about $80 an hour 🙁
    i might try get some blasting time at my old school. as for anodising,
    i cannot find anywhere that will do it and my anodising friend has left
    for Sydney.

    --
    tobbogonist

    Just Jake said:

    as long as youre not a total loser jock that gets mad when people arent
    "as good as you"


    ------------------------------------------------------------------------
    tobbogonist's Profile: http://www.unicyclist.com/profile/12176
    View this thread: http://www.unicyclist.com/thread/57702

  13. Aside from sandblasting there's a process I think is called "satin",
    where they have a cloth on a spinner (like a buffer) which will strip
    any paint or previous work to the metal. Though, the frame may be
    awkward to work with and they may not be able to reach all the areas.
    Also, if you get someone who's not really good with that machine they
    can 'eat' right into the metal if they hold too long or press too
    hard.

    You can get various colourings for your anodizing, but they all scratch
    fairly easily. For a more durable coating you would get a "hard
    anodizing". Someone said it before but I'll say again make sure you
    have them cover up any area where you don't want build up... like
    threads and whatnot.

    "Hard anodizing is a term used to describe anodic coatings with surface
    hardness and/or abrasion resistance as their primary characteristic.
    Great for surface to surface sliding with low loads The color of the
    natural anodic coating depends on the alloy and the coating thickness.
    e.g. 6061 has a tan or gray color which darkens to almost black at
    003"; 6063 has an amber shade which darkens to bronze. Both are
    considered clear. After hard anodizing surfaces may be sealed in
    boiling distilled water, sodium dichromate solution, dewatering oil,
    wax or PTFE solutions

    Class 1: Not dyed or pigmented.

    Class 2: Dyed. (Specify color on Drawing).
    Hard anodic oxide coatings find application in the engineering industry
    for components which require a very wear resistant surface. " Flash"
    hard anodize may be used instead of conventional anodize for corrosion
    resistance."

    [image: http://www.alexandriametalfinishers.com/pieces.gif]

    --
    thayr
    ------------------------------------------------------------------------
    thayr's Profile: http://www.unicyclist.com/profile/8957
    View this thread: http://www.unicyclist.com/thread/57702

Active in the last 60 minutes

Active in this thread

0 users · 0 guests ·0 bots ·0 total

No signed-in users are active right now.

No known search crawlers active right now.