Cycling Equipment · Public discussion

anodizing II

Started by Ant · · Last activity · 2 posts · 1,306 views

This thread is locked and is currently read-only.

Thread details

What we know about this thread

Original section
Cycling Equipment
Published
25 January 2003
Last activity
26 January 2003
Original author
Ant
Posts
2
Discussion status
Public discussion
Total views
1,306
Views / 30 days
0

The navigation and discussion metadata provide context. Posts remain in their original chronological order.

Showing posts 1–2 of 2
Posts remain in their original chronological order.

Text size
  1. I chanced upon the anodizing thread- actually, the un-anodizing thread with a link to anodizing
    instructions. this sounds pretty tempting, and as i will be making the odd aluminum part this
    spring, i thought i might give it a try. time permitting.

    does anyone know if anodizing changes the surface material? as in- if i machine a 27.2 mm seatpost,
    and anodize it, will it end up being
    27.1 mm? or 27.4? i am unfamiliar with the chemical/physical basis for the process, and would rather
    know before hand so i can compensate when i am making parts.

    or perhaps it changes nothing.

    thanks,

    anthony

  2. Anodising is the controlled formation of aluminium oxide at the surface of items made from aluminium
    and its alloys. When the coating is formed, it grows the surface by approximately 50% of the
    coatings thickness. Remember that this is per face, so component size growth will be X2 film
    thickness for a diameter.

    If the coatings are thin (i.e. less than 10 microns) or the application is not dimensionally
    critical, then this effect can be ignored.

    Check out acornhardas.co.ukdatasheets.htm this is a company I used to work for, who
    pretty much invented hard anodising back in something like 1920.

    Paul

    "ant" <[email hidden]> wrote in message
    "]news:[email hidden]...

    Quoted message said:

    I chanced upon the anodizing thread- actually, the un-anodizing thread with a link to anodizing
    instructions. this sounds pretty tempting, and as i will be making the odd aluminum part this
    spring, i thought i might give it a try. time permitting.

    does anyone know if anodizing changes the surface material? as in- if i machine a 27.2 mm
    seatpost, and anodize it, will it end up being
    27.1 mm? or 27.4? i am unfamiliar with the chemical/physical basis for the process, and would
    rather know before hand so i can compensate when i am making parts.

    or perhaps it changes nothing.